Choosing a tag that survives −40.
Can Alta is Canada’s largest manufacturer of health and safety tags. A tag fails in one of three ways: it snaps, it fades, or nobody can read what was written on it. All three are decided at the specification stage, and all three get worse below about −25°C. Here is how to specify a tag that is still doing its job in February.
Why paper and card are not candidates
This seems obvious until you see how often it happens. Card tags get used because they were on hand, and then a chinook cycle takes the site from thaw to deep freeze in a day, the card absorbs water, freezes, and tears at the hole the first time somebody tugs it.
Even laminated card fails, and it fails worse, because the lamination traps the moisture that got in at the cut edge. If a tag is going outdoors in Alberta, it needs to be a plastic tag from the start.
Polyethylene, and why thickness is the decision
We run tags in polyethylene stock, principally .023″ and .035″. Polyethylene is the right family for this because it stays flexible when it is cold instead of becoming glassy and brittle — and brittleness is what actually kills a tag, because the failure happens at the grommet where the stress concentrates.
The choice between the two thicknesses is mostly about handling, not about weather:
- .023″ — the general-purpose thickness. Right for tags that hang undisturbed, are handled occasionally, or are replaced on a cycle. Most inspection and identification tags.
- .035″ — noticeably stiffer. Right where the tag is handled constantly, where it will be flexed against an edge, where it hangs off equipment that vibrates, or where it simply has to stay on a valve for a long time without anyone tending to it.
If you are between them and the tag is going outdoors on something that moves, go heavier. The cost difference per tag is small; the cost of a re-tag trip to a remote site is not.
The grommet is the failure point — size it deliberately
Almost every tag that fails in service fails at the hole. Two things prevent that: the right material (above) and a grommet that matches what is going through it.
Grommets are specified by inside diameter, and the two we use most are #00 at 3/16″ and #2 at 3/8″. Before you order, find out what will actually attach the tag. Wire and standard zip ties pass through 3/16″ comfortably. Heavy cable ties, S-hooks, beaded chain and carabiners often will not — and a tag whose hole is too small for the hardware on site gets attached with whatever is to hand, badly.
The other half of this is placement. A grommet set too close to the edge tears out under load no matter how good the material is. Leave real margin between the hole and the edge of the tag, and if the tag will hang under any weight or be tugged repeatedly, consider a reinforced or double-grommet layout.
Design the writing surface for a gloved hand
Most industrial tags are filled in by hand, outdoors, by someone wearing gloves. That is the design brief, and it rules out a lot of what looks good on screen.
Write on light, print on dark. Reversed-out white text on a saturated background photographs beautifully and cannot be written on. Keep the fill-in areas light and unprinted.
Rule the lines and make them big. A field sized for neat indoor handwriting will be overrun in the field. Assume block capitals from a gloved hand with a marker.
Say what goes in each field. A tag with unlabelled blank lines gets filled in inconsistently, and inconsistent records are the ones that fail an inspection.
Colour-code by state, not by department. The colour should tell somebody at a glance whether they can proceed. Anything else the colour is being asked to do is competing with that.
The service-life question, answered honestly
You will be quoted outdoor service-life figures for tag material. We do not publish one, because there is no standard test behind those numbers and the honest answer depends on UV exposure, abrasion, chemical contact and how often the tag is handled — variables that differ by an order of magnitude between a valve tag inside a building and one on a wellhead.
What we will tell you: polyethylene tag stock stays flexible in Alberta cold, tolerates the hydrocarbons and solvents common on industrial sites, and does not delaminate when wet. Screen-printed ink on polyethylene outlasts anything written by hand on the same tag, which means the printed structure of your tag will still be perfectly legible after the handwriting has weathered. That is worth knowing when you decide what to print and what to leave blank.
Tag specification quick reference
- Stock
- .023″ polyethylene (general purpose) · .035″ polyethylene (heavy handling, vibration, long service)
- Why polyethylene
- Stays flexible in deep cold instead of going brittle — brittleness at the grommet is the usual failure
- Grommet inside diameter
- #00 = 3/16″ · #2 = 3/8″
- Attachment check
- Confirm wire, tie, hook or chain diameter before choosing the grommet
- Writing areas
- Light background, ruled, labelled, sized for block capitals from a gloved hand
- Decoration
- Screen printing — the printed structure outlasts the handwriting on the same tag
Answered, briefly.
What material should an outdoor tag be made from in Alberta?
Polyethylene tag stock. It stays flexible in deep cold rather than going brittle, and brittleness at the grommet is how cold-weather tags actually fail. Card and laminated card are not suitable outdoors here — laminated card is worse, because the lamination traps moisture that entered at the cut edge.
What is the difference between .023" and .035" tag stock?
Stiffness and handling tolerance rather than weather resistance. Use .023″ for tags that hang undisturbed or are replaced on a cycle, and .035″ where the tag is handled constantly, flexed against an edge, mounted on something that vibrates, or expected to stay put for a long time without attention.
What size grommet do I need?
Grommets are specified by inside diameter. A #00 is 3/16″ and a #2 is 3/8″. Choose based on what will physically attach the tag — wire and standard zip ties pass 3/16″ comfortably, but heavy cable ties, S-hooks, beaded chain and carabiners often need 3/8″.
How long will an outdoor tag last?
There is no honest single number, and we do not publish one. Service life depends on UV exposure, abrasion, chemical contact and handling frequency, which vary enormously between applications. Any supplier quoting one figure for all outdoor use is guessing.
Why does the writing on our tags become illegible?
Usually because the fill-in area was printed dark or reversed out, or was sized for indoor handwriting. Keep writing fields light and unprinted, rule them, label them, and size them for block capitals written with a marker by a gloved hand.
Can you print our own tag design?
Yes — tags are made to your artwork in our Canadian plant, screen printed, with your choice of stock, grommet, size and colour. Every order includes a free electronic proof before anything is printed.
Talk to the people who make it.
We have manufactured in Canada since 1974. Tell us the application and we will specify it properly — including telling you when the cheaper option is the right one.